Well i used fleece for my door pods. i used about 1/2 gallon of resin on the 2. (and man that f@cker was wet.)

Now I have a problem. Part of the mold is alittle soft what do I do?

Do I just add some more resin till it gets hard?

Or do i have to redo it all ? (I hope not)

 
Well I put some more on the weak spot and waited about 20 minutes and it is hard as a rock.

I stood on it and even bounced. I am 185 pounds and it didnt even flex.

Now time to add a few layers of glass.

 
Activity
No one is currently typing a reply...
Old Thread: Please note, there have been no replies in this thread for over 3 years!
Content in this thread may no longer be relevant.
Perhaps it would be better to start a new thread instead.

About this thread

2loud4u

10+ year member
Nothing to see here
Thread starter
2loud4u
Joined
Location
canada
Start date
Participants
Who Replied
Replies
1
Views
434
Last reply date
Last reply from
2loud4u
IMG_0710.png

michigan born

    May 14, 2026
  • 0
  • 0
IMG_0709.png

michigan born

    May 14, 2026
  • 0
  • 0

New threads

Top