It's easy......
Put the mold in the machine, throw pewter, zinc or whatever metal it is(600+ degrees, it burns:fyi

throw it in the spinning machine, centrifugal force takes over by spreading teh liquid metalz into teh mold, take it out teh mold, let it cool off, cut the excess material and throw it back in the tank to melt, then take the product into the BOOTH OF HELL, throw em in a basker, dip em in hot soapy water, then into 2 separate tanks of water, then into teh Ac1Dzorz, then into another 2 separate tanks of water, then into a basket, then they go into a 25hp dryer:naughty: for 5 mins, put em in a basket, grind the excess shit off and the sides, then polish em, then paint, then package em, then Teh UPS takes em
I was doing some for some Louisiana Literary Run or some shit...