nismboy6986
10+ year member
the **** technician
- Thread Starter
- #16
but does that stuff have any work time since my enclosure makes the transition from horizontal and flat to vertical and round pretty sharply and i would need time to work out the wrinkles. sound like i will be using super 90 then. the stuff we use at work is red. we just do shelves and shit for stores. i personally would buy any of that crap for the price they charge. (its just melamine and then how we basically just use crayons to fix chips in laminate ect)